I've been re-exploring the black sands rabbit hole recently, and figured I'd share my recent understandings.
I've already visited Larry Blackman's (aka "the essene") path of extracting precious metals from black sand on THIS thread.
Here's the recap:
There's also John Milewski's process of extracting gold from black sand (and glass), which was talked about on THIS post.
Here's the recap:
Here's a youtube video showing how to pull gold from black sand using fire assay:
Joe Champion, said in THIS book (which also talked about extracting precious metals from black sand), that you can increase the yields by pre-treating.
He specifically mentioned the following treatment options discovered by other people:
The idea of pulling gold out of black sands isn't controversial in and of itself.
Gold prospectors routinely process their black sands to recover hidden particles of gold, such as described HERE.
But the yields significantly vary from different sources.
This variance in recovered gold from various sources of black sand reminds me of Vinny Pintos comments [Link HERE]:
In both cases, I've long suspected that repeated cycles of freezing/thawing might be charging the internal HIM portion thereby improving the results.
Unfortunately Vinny never said which areas produce better performing magnetite.
But WRT gold from black sands, it's quite obvious that it's in the colder areas of Australia and New Zealand which regularly dip below freezing where more fine particle gold is found within black sands.
We already know from Reich's work on bion packs that regular freeze and thaw cycles cause various substances to induce healing, and it's assumed that the same process will 'charge' life-force containing water.
I recently assumed that doing freeze/thaw/heat cycles to black sands would further increase the amount of gold recovered in the same way as the other techniques described by Joe Champion.
In fact WRT the Milewski process, that's exactly what I think is happening..Eg: each heat and cool repetition is simply 'charging' the HIM portion of the black sands, so when the final fire assay is performed, it maximises the transmutation power within the black sands.
I had figured that I wanted to test this out by running my own cycles of freeze + heat on black sands, followed by Joe's ball mill process before testing out with a fire assay. I was hoping that this might get very close to Joes' mythical maximum of 10% precious metals from fire assay.
But then we had @Vladimirv join the forums and shared his excellent research about producing ORMUS gas HERE.
In his first ever post to the forums he said:
Anyway, just sharing these musings in case they resonate with anyone else.
I've already visited Larry Blackman's (aka "the essene") path of extracting precious metals from black sand on THIS thread.
Here's the recap:
here’s how I think The Essene was making his gold:
> Perform a lye burn on the black sand from the mine tailings
> Precipitate the ormus white powder metals
> Dissolve the white powder in hydrochloric acid and discard what doesn’t dissolve
> Precipitate the white powder metals back out of hydrochloric acid, then separate out and dry (should be white powder of iridium and gold)
> Mix the dry white powder with sulfur and burn
> Add silver to the white powder and sulfur and melt them all together
> After cooling, place the entire mass in nitric acid to dissolve the silver out (and vapor off remaining sulfur as SO2)
> Remove the remaining solids and put them in aqua regia (this will be gold + iridium metals)
> Remove the remaining solids and melt into a bar (will be iridium metal which doesn’t dissolve in aqua regia)
> Precipitate gold out of the aqua regia, separate it out and melt into a gold bar
> There will probably also be a small amount of platinum dissolved in the remaining solution, which can also precipitate, separate out and melt into a platinum bar.
There's also John Milewski's process of extracting gold from black sand (and glass), which was talked about on THIS post.
Here's the recap:
The John Milewski process never specifically described how to get the metallic gold out of the final result, but John said several times in lectures that he used fire assay.Just in case these links/videos ever go bad, I'll briefly describe here:
> Wet grind beer bottle glass in hammer mill
> Add magnetite sand and powdered charcoal (or graphite) to the ground glass and water slurry
> Put the mixture into a microwave oven crucible + furnace and fire it up
> Remove from furnace and quench pour the molten slurry into a container of water
> Take the solidified glass mixture and repeat furnace and quench stages to increase yield (John says 10 - 20 times)
> regrind the glass mixture and extract the gold using conventional hydrolic methods (or apparently can also use fire assay technique)
Here's a youtube video showing how to pull gold from black sand using fire assay:
Joe Champion, said in THIS book (which also talked about extracting precious metals from black sand), that you can increase the yields by pre-treating.
He specifically mentioned the following treatment options discovered by other people:
Joe also discussed in detail the following treatment option (which was discovered by himself):the first common denominator was they directly treated the black sands. And second, each used a high temperature digestion process.
The following is a typical description of their processes:
Don Jordon: NaOH + H202 (sodium hydroxide + hydrogen peroxide). Compound is mixed with the mineral, then fused.
Greg Iseman: 3HC1 + HN03 + HF (Modified Aqua Regia) .
The solution and mineral is placed in an industrial microwave until dissolved.
Beckman Laboratories: Acid Bomb. The mineral is mixed with a flammable chemical constituent, then placed within a high pressure container and ignited by a spark.
For small batches, all that is required is an enclosed laboratory ball mill and black sands. I would recommend Denver Laboratory Ball Mills which are readily available. The black sands used in our tests came from desert deposits outside of Buckeye, Arizona and other sands magnetically separated from rich mineralized copper deposits in New Mexico. The ball mill should be of such design wherein it is completely sealed and has a metallic liner. The balls must be made of non-coat carbon steel. New Teflon coated material will not work. As in the case of the Denver Laboratory mill we used, we had 11.91 kilograms of steel balls with diameters ranging from approximately one-half to 3 inches. We used 2.5 kilograms of black sands. Seal the container and operate for no less than 6-8 hours without interruption. open and take a representative sample of 50.0 grams. Place in sizing screens. If +70% of the material passes through a 200-mesh screen, then remove all the material from the ball mill. However, if the aggregate particle size is greater than 200-mesh, replace the black sands in the mill and operate for an additional 6-8 hours, repeating the same steps. A note of importance. The minimum six hour continuous operation is an extremely important criteria. With operation of three hour intervals, numerous failures have occurred. Wherein operating a continuous +6.0 hours we have yet to see a failure in the production of precious metals....After extensive pulverization(6-8 hours), a significant "nuclear change" occurs within the ball mill. Significant in the fact that by weight 0.5% to 10.0% of the original black sands was converted to precious metals.
The idea of pulling gold out of black sands isn't controversial in and of itself.
Gold prospectors routinely process their black sands to recover hidden particles of gold, such as described HERE.
But the yields significantly vary from different sources.
it depends on gold concentration in the black sand. I had recovered 2.8 grams of gold from 420 grams of black sand from one location. And I got no gold from 340 grams of black sand from different location.
This variance in recovered gold from various sources of black sand reminds me of Vinny Pintos comments [Link HERE]:
Even though Vinny was talking about using magnetite for MEOW devices, and Joe was talking about increasing yields from gold extraction from magnetite, for a long time I have wondered if they are not due to the same cause.All Magnetite Sands Are Not Created Equal
As noted elsewhere on this site, a number of us have found that when using magnetite sand for the purposes of constructing MEOW devices and similar technologies, not all magnetites are created equal, and rather, it seems that there is considerable variance in effectiveness or power across batches and types of magnetite sand.
In both cases, I've long suspected that repeated cycles of freezing/thawing might be charging the internal HIM portion thereby improving the results.
Unfortunately Vinny never said which areas produce better performing magnetite.
But WRT gold from black sands, it's quite obvious that it's in the colder areas of Australia and New Zealand which regularly dip below freezing where more fine particle gold is found within black sands.
We already know from Reich's work on bion packs that regular freeze and thaw cycles cause various substances to induce healing, and it's assumed that the same process will 'charge' life-force containing water.
I recently assumed that doing freeze/thaw/heat cycles to black sands would further increase the amount of gold recovered in the same way as the other techniques described by Joe Champion.
In fact WRT the Milewski process, that's exactly what I think is happening..Eg: each heat and cool repetition is simply 'charging' the HIM portion of the black sands, so when the final fire assay is performed, it maximises the transmutation power within the black sands.
I had figured that I wanted to test this out by running my own cycles of freeze + heat on black sands, followed by Joe's ball mill process before testing out with a fire assay. I was hoping that this might get very close to Joes' mythical maximum of 10% precious metals from fire assay.
But then we had @Vladimirv join the forums and shared his excellent research about producing ORMUS gas HERE.
In his first ever post to the forums he said:
I've taken this post and experimental results as a nice little wink from the universe. Thank you @VladimirvBefore working with ORMUS-containing sources containing large amounts of ORMUS particles, such as azomite, natural Dead Sea salt, sea salt, iron ore magnetite, rock oil mineral, Himalayan pink/black salt, gold or silver ore, it is useful to activate them by exposing them to a pulsating magnetic field, cyclically calcining them at 250-300 degrees Celsius, then boiling them in water and freezing them. Then, grind them for a long time in a ball mill.
Anyway, just sharing these musings in case they resonate with anyone else.