Gold from Black Sands

Dendritic Xylem

Invenies
Honorable Meister
Hermetic Pilgrim
Joined
Mar 1, 2010
Messages
621
Unfortunately I met with a couple of problems trying to separate the gold from the bismuth.
Of course, I also need to determine the easiest way to get the gold out.

It's extremely easy to separate gold from bismuth with a cupel, or parting with nitric or even hot concentrated sulfuric. I don't understand why you would assume you have gold when you still haven't actually separated the gold. Feeling the weight of a bismuth button in your hand isn't a good test. How would you know it's gold instead of another heavy metal like platinum? Unless the button has a yellowish color from very high concentration of gold. Also, it's well known in the mining industry that having sulfur in a smelt complicates the extraction of gold. The sulfur forms a speiss layer that captures gold. This is why most people go to so much trouble to remove sulfur by roasting the material before smelting/assaying.

I know you're going off Jason's (Mount Baker Mining and Metals) experimental use of NaOH to deal with sulfides. But you need to remember he's running very high yield mining concentrates rather than low-grade raw materials like you. It makes a big difference.

Maybe adding sulfur in the form of copper sulfate helps with transmutation. But it can reduce yields if the only part you keep is the collector metal button. I'm not trying to be a dick. I hope your assumptions are correct. But they are still just assumptions until you have the separated gold in hand.

If the sulfur smelts cause problems and you don't find gold in the button, it might be worthwhile to try two smelts with a roasting step in between. Do the first melt without collector metal. Then crush the melted material into a powder. Gently and slowly roast this powder in a shallow dish open to the air while occasionally stirring it with an iron or graphite rod, until all the sulfur has been removed. If you roast too aggressively (too hot too fast) some of the gold can actually be lost into the air. Now take your roasted powder and do another smelt with collector metal. It might require additional flux. Now part the button with a cupel or acids.

If you decide to use copper as a collector, make sure you melt in a reducing environment without oxygen. Otherwise much of the copper will oxidize and go into the slag. Unless you use metallic iron for reduction. But I think that can cause other problems.

I hope it works out for you! :)

DISCLAIMER....NITRIC ACID RELEASES TOXIC GASES AND HOT CONCENTRATED SULFURIC DISSOLVES SKIN VERY FAST.
ANYONE THAT TRIES THIS SHOULD USE PROPER VENTILATION AND PROTECTIVE GLOVES AND FACE SHIELD.
THE SMELT WITH SULFUR ALSO NEEDS GOOD VENTILATION DUE TO TOXIC SULFUR GASES.
 
Last edited:

ghetto alchemist

Hermes Trismegistus
Honorable Meister
Hermetic Pilgrim
Joined
Mar 21, 2011
Messages
1,537
Moray specifically described that bombardment by electron beam, x-ray radiation, or laser light into a solution of the ore will massively improve the yield of a low yielding ore (curiously he also said that these processes will only marginally improve a high yielding gold ore).

So at a minimum, you could expect that either of those 3 processes would also improve the M3 yield from magnetite black sand.
IMO you could also expect that strongly heating in a microwave oven would do the same.
Just wanted to update with some recent discoveries.
Earlier in this thread I hypothesised that the 3 processes discovered by Moray were simply energising the magical HIM component within the ore causing it to transmute more precious metals, and that using a microwave oven should do the exact same thing but is more accessible for the average person.

So for anyone wanting to replicate please make sure to pre-energise your magnetite the same way.
I think the easiest way to do it is to alternate between freezer time and putting in a microwave oven.
In another thread I hypothesised that alternating between freezer time and a microwave over would be a good way to energise the HIM component (this was in regards to increasing the healing capacity according to the bion pack process).
In that regard putting in a microwave is a 2-for-1 deal because plain heating works, and with a microwave you get both straight heating of magnetite along with exposing it to energising radiation.

If synthesizing commercial amounts of gold was that easy, the process wouldn't have flown under the radar.
It turns out that these kinds of techniques are indeed being used commercially by various actors, they're just not telling you they're doing it.
See this paper:
[LINK] Due to the special characteristics of pyrite cinder, the gold and silver in it can be locked by other minerals. Therefore, techniques such as activation methods can be applied to expose these metals to a leaching reagent or other process. The activation can be undertaken using mechanical, thermal, biological, ultrasonic, and chemical methods
....
References: Innovative Methods for Intensifying the Processing of Zinc Clinker: Synergy of Microwave Treatment and Ultrasonic Leaching.
In the the paper, the author says that it is known that certain physical processes on the ore (prior to leaching) will improve precious metals yields.
The author doesn't specifically mention microwaving the ore (perhaps it's a bit controversial still), but he does link to another paper in the references showing that treatment in a microwave improves zinc yields.

[LINK] The Essene also would microwave his precipitate before mixing with silver and heating the entire mass in an induction furnace.
And I just came across a recent historical reference that the Essene was also processing his precipitate in a microwave in order to improve yields.

Vindicated.
 

ghetto alchemist

Hermes Trismegistus
Honorable Meister
Hermetic Pilgrim
Joined
Mar 21, 2011
Messages
1,537
Another thing I came across recently, which I think is relevant to the thread...

If you check THIS ebay listing selling magnetite, it says:
Others have claimed gold extraction from the black sands after crushing them further than the 30 minus size they are now.

I found it interesting because it shows that some people are indeed taking advantage of the techniques described in this thread for gold production.
It doesn't mention pre-energising the magnetite (but IMO they'd be stupid not to do it).
However, crushing the magnetite into smaller grain sizes is very much in line with this thread (IMO it kick starts the popcorn reaction by exposing the internal HIM inside the magnetite to any external sulfur).
 

Mahavira

Terrae
Hermetic Pilgrim
Joined
Apr 4, 2024
Messages
295
From reading your last couple posts, it occurred to me once again that anything that seems to be an "enemy" to the ormus/m-state, like sulfur, EM/microwave radiation, the sun, etc, seems to be in an inversely proportional way a "friend" to metal yield. Like the more the "enemies" are used on the m-state the more it reverts back to metal.

The same would apply to any matter naturally loaded with HIM/prana like magnetite. So microwaving it in addition to all the other treatments would essentially further convert it's m-state HIM rich part to their metallic counterparts.

If this line of thought is correct it would mean that microwaving magnetite to breathe the PRAGG straight would not be a good idea because then there would be the risk to also maybe breathe in heavy metal gases not yet fully converted to solid metals.
 

Vladimirv

Terrae
Hermetic Pilgrim
Joined
Dec 7, 2025
Messages
152

This guy claims that prolonged processing of graphite powder in a ball mill with zirconia ceramic balls causes the graphite to become magnetic.

A few years ago, I came across a claim on a forum where someone used quartz balls and small natural quartz crystals to grind the starting materials in a ball mill. He claimed that this type of grinding produces the greatest effect for transmutation. He tried to replicate D. Champion's experiments. Grinding with metal balls, he said, is very ineffective.

I think that quartz and zirconia ceramics create micro-discharges of static electricity when they collide because they have a piezoelectric effect. This charge is transferred to the particles of the materials being ground, activating the ORMUS particles there. These micro-discharges can also convert metal nanoparticles from their metallic form to the ORMUS form. If the material is sufficiently dry (D. Champion emphasizes this point in his book), it becomes additionally electrified during grinding due to friction.

As a result, prolonged processing can result in both the activation and growth of existing ORMUS particles in the material being ground, as well as the production of new ORMUS particles.
 

ghetto alchemist

Hermes Trismegistus
Honorable Meister
Hermetic Pilgrim
Joined
Mar 21, 2011
Messages
1,537
From reading your last couple posts, it occurred to me once again that anything that seems to be an "enemy" to the ormus/m-state, like sulfur, EM/microwave radiation, the sun, etc, seems to be in an inversely proportional way a "friend" to metal yield. Like the more the "enemies" are used on the m-state the more it reverts back to metal.
There's a problem with this idea, and that's the fact that so many people use a microwave oven for heating food.
I personally cook with a microwave for most meals.
If what you say is true, then people who regularly use a microwave oven should produce clusters of heavy metal poisoning, because so-called ormus elements were well proven to be in many food sources.
But it's not true at all.
Even after decades of microwave ovens being used for cooking, there is absolutely no data that suggests the food is tainted in any way nor that there are any long term negative health consequences of any kind.
I had a friend who once tried to tell me that he strictly avoids using them because they eject the life-force out of food.....but again, if that were true then I should have been at sub-optimal health (compared to people like him) from using one so extensively in the past, but I never have been (even before I deliberately started ingesting strong prana substances).
Ironically, he was the one who later got cancer.

The same would apply to any matter naturally loaded with HIM/prana like magnetite. So microwaving it in addition to all the other treatments would essentially further convert it's m-state HIM rich part to their metallic counterparts.
Because of what I wrote above, again I don't believe that.
I think you'd have to agree that ALL of the reactions which we know of that convert the prana substances into metal involve the presence of sulfur in some form (which is the basis of popcorn theory).
TBH I'm not comfortable with this myself.
But I had to go there, because that's where the science leads.
Until you can find someone who was able to turn prana substances to metal without any sulfur present, IMO it's a fact that the metal creation reaction is only initiated by sulfur and nothing else.

If this line of thought is correct it would mean that microwaving magnetite to breathe the PRAGG straight would not be a good idea because then there would be the risk to also maybe breathe in heavy metal gases not yet fully converted to solid metals.
I'll admit that it is a possibility that processing a raw magnetite ore into a medicine and then ingesting it would be very dangerous for potential heavy metal poisoning, because of the possibility of lead or mercury contaminants in the magnetite.
This is EXACTLY the reason why I created the PRAGG, was to avoid this possibility. By breathing in a gas, you leave the heavy nasties behind.
IMO bubbling through lye and water is a further protection for any unwanted vapours in the gas.
So it's irony to me that you're highlighting the PRAGG as posing the exact danger that it was created to avoid. :p
 

ghetto alchemist

Hermes Trismegistus
Honorable Meister
Hermetic Pilgrim
Joined
Mar 21, 2011
Messages
1,537
A few years ago, I came across a claim on a forum where someone used quartz balls and small natural quartz crystals to grind the starting materials in a ball mill. He claimed that this type of grinding produces the greatest effect for transmutation. He tried to replicate D. Champion's experiments. Grinding with metal balls, he said, is very ineffective.
Interesting research there.
I don't suppose you have a link to that forum by any chance?
 

Vladimirv

Terrae
Hermetic Pilgrim
Joined
Dec 7, 2025
Messages
152
Interesting research there.
I don't suppose you have a link to that forum by any chance?
This is an old Russian-language forum. It's been abandoned for about five years, and the site's engine isn't working. I've basically described everything from memory. There's no other valuable information there.
One of the participants, during a discussion of D. Champion's experiments, wrote that he tried to replicate his recipes from the book and that the best results were achieved by grinding metal salts in a ball mill with quartz balls and crystals for 2-3 days. As far as I remember, he didn't manage to get the 10% that Champion got. The results were much lower.
 

Mahavira

Terrae
Hermetic Pilgrim
Joined
Apr 4, 2024
Messages
295
If this line of thought is correct it would mean that microwaving magnetite to breathe the PRAGG straight would not be a good idea
So it's irony to me that you're highlighting the PRAGG as posing the exact danger that it was created to avoid. :p
My mistake, That was a typo. I meant to say breathe the Prana Gas, PRAG, in general, not speaking about the Prana Gas Generator, PRAGG, specifically.
 
Last edited:

Mahavira

Terrae
Hermetic Pilgrim
Joined
Apr 4, 2024
Messages
295
I had a friend who once tried to tell me that he strictly avoids using them because they eject the life-force out of food
I agree 100%. Lucky it didn't affect your health as much. But still IMO you'll feel even better and stronger without it.
 

Vladimirv

Terrae
Hermetic Pilgrim
Joined
Dec 7, 2025
Messages
152
To initiate the transmutation of one metal into another, medieval books say you need to take the first part of ORMUS from the earth/ore, and the second part from the air/dew/stormwater. There are also similar options for catching ORMUS from the air using traps like this one.



There's a book by the French author François Jollivet-Castelot called "How to Become an Alchemist: A Treatise on Hermeticism and Spagyric Art Based on the Keys of the Tarot."
It describes the alchemical experiments of August Strindberg.

Link to the French original

Link to the English translation

He describes several recipes and outlines his theory. It almost completely coincides with that put forward by D. Champion (Arephmetic addition of atomic weights of chemical elements in molecules.). I highly recommend reading it.
Essentially, it describes recipes for isolating ORMUS particles from air and metal salts on the surface of an aqueous solution in the form of an oily film. This ORMUS is then activated using sulfur obtained from the smoke of a lit cigar.


page . 259
Quote.

Experiment III – Simplified Method for Larger Yield
In a tub, combine:
• 1 part copper sulfate
• 3 parts iron sulfate
• Ammonium hydrochloride
• Ammonia (quantity as desired)
Fill the tub with water and let it rest in the sun or near a fire.
After a few hours, or better yet, after a day, greasy spots will appear on the water's surface. Skim these
spots onto paper and let them dry very gently. By occasionally adding more ammonia, production
can continue for weeks.

If you place this solution in a sealed plastic container with thin glass and add ammonia, you can collect ORMUS without wasting ammonia or creating a strong odor. ORMUS in its volatile plasma form easily penetrates the thin plastic of water bottles.
You can also add electrodes and a high-voltage capacitor (5-10 kV) to further attract ORMUS from the air into the bottle.
 

Mahavira

Terrae
Hermetic Pilgrim
Joined
Apr 4, 2024
Messages
295
So I finally gave up the idea and decided to try another smelt with copper instead of bismuth
After an internet search, it seems separating gold from copper is more difficult than gold from bismuth. For the latter if one used nitric acid (at a concentration of 30% or so) to dissolve the bismuth, gold stays behind as a solid. And bismuth can be recovered at about 90/95% by a relatively simple process.

What type and size of ball mill do you use please?
 
Last edited:

ghetto alchemist

Hermes Trismegistus
Honorable Meister
Hermetic Pilgrim
Joined
Mar 21, 2011
Messages
1,537
What type and size of ball mill do you use please?
I was just using a standard paint can with plain steel balls maybe 4-5mm diameter.
After an internet search, it seems separating gold from copper is more difficult than gold from bismuth. For the latter if one used nitric acid (at a concentration of 30% or so) to dissolve the bismuth, gold stays behind as a solid. And bismuth can be recovered at about 90/95% by a relatively simple process.
Yeah, this thread is due for an update, I've just been putting it off, but I'm taking this as a sign that it's time.
Firstly, yes..you're right, just as dendritic xylem said, a straight dissolve in nitric acid easily removes the bismuth.
It doesn't take too long and doesn't even require any external heat... but even so I still having problems which I'll get to in a second.

Secondly, yes indeed just as you say, bismuth is a far better collector metal than copper, which is garbage.
Don't use copper, just use bismuth.

Thirdly, yes it easy to separate gold from bismuth, exactly as you say.....as long as you're not me.

The method described in this thread is THE BOMB... last run I did, I carefully weighed and used 100g of bismuth on a smelt on 400g of black sand.
And I got a button of 149g, of which should have had approximately 12g of copper from the decomposing of the 50g of copper sulfate, leaving 37g of new metal.
Unfortunately it's not all gold, but mostly silver with a bit of gold.
But even if it's all silver, this process will still be profitable.
That's basically a whisker under 10% yield, which is the maximum result that Joe champion was talking about as possible to produce.

But even so, I keep having persistent bad luck recovering the gold, so much so that I just left the whole kit out in the weather untouched for the past week out of pure exasperation.
The bismuth button dissolved with no problem in 300ml nitric acid leaving some black powder in the bottom of the beaker (as expected), and likely was gold.
But as soon as dusk hit, the air temperature dropped (currently winter here in australia), the solution got chilled and dropped out crystals everywhere as I was halfway through filtering it.
I left it sit out overnight and then added water to everything the next morning to try to redissolve the crystals, and it made white precipitate drop everywhere including inside the filter paper (likely silver chloride due to chlorine in the water).
I was so gutted by these mistakes, because the next step was an easy gold recovery by burning the filter paper in an oxy-propane flame, but now it's contaminated with silver.
Then I walked away, and haven't returned to it since.
[I swear, it feels like the universe is very happy for me to tell all you good people all about this, but is totally opposed to me doing it myself. :p ]
In short, bismuth and nitric acid should easily work to get the gold....
[Eg. Smelt BS with bismuth, dissolve the button in nitric, filter out gold and burn paper into a button, then cement out your silver, filter and melt the silver into a button]
Just don't be a muppet like me, and let the solution get chilled, half way through processing it.
And even more important, don't add chlorine containing water at any stage while you're processing it.

I suppose on a positive note, this is a good time for me to wrap up my public involvement with this process.
Yes, ghetto's shit is good....the process laid out in this thread makes bucketloads of precious metal [see post #25, and pretreat the magnetite with multiple times freeze and heat in microwave, ball milling not even required because the lye does the same thing by partially digesting the BS during the smelt]..
But no, I can't tell you exactly how much gold it gets, because I still simply don't know.
But....I don't think I'll be comfortable to report that information anyway, even after I find out.
So I leave it here...IMO everyone should be working on this process, tweak the different variables to find the way to get less silver and more gold
(I suspect that it might simply require longer smelt time).
But I also know that almost nobody will, and that's probably a good thing.
Perhaps you might be the only one @Mahavira .....
 
Last edited:

Pilgrim

Hermes Trismegistus
Hermetic Pilgrim
Joined
Apr 26, 2023
Messages
1,257
After an internet search, it seems separating gold from copper is more difficult than gold from bismuth. For the latter if one used nitric acid (at a concentration of 30% or so) to dissolve the bismuth, gold stays behind as a solid. And bismuth can be recovered at about 90/95% by a relatively simple process.

Poster @nav2010 made a few posts about the maths/science of transmuting metals.

Gold atomic number is 79 so has 79 protons

Silver atomic number is 47

Getting from one element to another requires the addition or subtraction of the necessary number of protons. In domestic chemical terms we can only deal in certain elements to add or subtract due to how stable or unstable they are.

Generally speaking, reactions that use Oxygen (8) or Carbon (6) or Nitrogen (7) are likely the ones that ordinary people will be able to use.

So when you consider how to get from some base metal/element to Gold (79) or Silver (47) then you have to think in terms of multiples of 6, 7 or 8 (to use Oxygen, Nitrogen, Carbon molecules).

So let's look at an easy one. Silver to gold.

Silver is 47, Gold is 79 so the difference in a nice round 32 protons and that of course is exactly 4 x Oxygen (8) molecules.
How can you add 4 Oxygen molecules to silver? Well I don't know the process but Nav convinced me that the Singlet Oxygen molecule is the key to much of the transmutation work and so using Ozone in the process would be an easy way to get those 4 singlet Oxygen molecules. Ozone is O3 of course so if you're putting Ozone into the process then O2 molecules will easily bind to Hydrogen to create water and leave a spare O molecule. This I think is where the secret lies. Singlet Oxygen. Ozone.

Another interesting fact is that Stibium, better known as Antimony has atomic number 51.

To get from 51 to Gold (79) is exactly 28 protons. That's another neat number. It could be 2 x Oxygen (8) and 2 x Carbon (6)
i.e. Antimony (51) plus 2 x Oxygen (16) plus 2 x Carbon (12) = 79 Gold.

So what about Bismuth which was mentioned in your post?

Bismuth is atomic number 83

Difference between that and gold (79) is 4 which would be a Berylium molecule. Not sure I know any processes that use Berylium.

Ok so how about Silver?

Bismuth 83, Silver 47, the difference is 36

36 could be 3 x Oxygen(24) and 2 x Carbon (12)

So it would not surprise me in the least that there might be an easy way to process Bismuth and lose 3 oxygen molecules and 2 carbon to get Silver. Ghetto in his post confirms that he got "mostly silver with a bit of gold." so there you go.

Why would Copper be difficult to use?

It's atomic number is 29

Gold 79 minus Copper 29 is a difference of 50

50 doesn't carve up nicely with Oxygen(8) and Carbon(6) molecules. I think the only way is 7 Carbon (42) and 1 Oxygen (8)
but I don't know any process to easily generate specifically 7 molecules of carbon when you also want 1 molecule of Oxygen.
I presume if you tried using Ozone and some Carbon related compound the Singlet Oxygen molecules, being so "hungry" to bind to anything would get there first and so you'd quickly have more than 1 Oxygen molecule binding and thus never get to your perfect 50.

If I were going to do any such work (and I haven't nor am I in any position to do so) I would begin with Silver and try and find a process that incorporates Ozone with it in order to simply add 4 Singlet Oxygen molecules in order to get Gold. No idea if that's possible but clearly this is the math of it all. Its all about adding or subtracting protons by using readily available elements.
 

ghetto alchemist

Hermes Trismegistus
Honorable Meister
Hermetic Pilgrim
Joined
Mar 21, 2011
Messages
1,537
the process laid out in this thread makes bucketloads of precious metal [see post #25, and pretreat the magnetite with multiple times freeze and heat in microwave, ball milling not even required because the lye does the same thing by partially digesting the BS during the smelt]..
but I don't know any process to easily generate specifically 7 molecules of carbon when you also want 1 molecule of Oxygen
Ahh...you just reminded me of one very small detail.... there is one ingredient which I add to the smelt which I didn't mention.
And that is a sprinkle of flour, not much....I only do so because other fire assay receipes say that a tiny bit of flour becomes carbon which improves yields, and since Milewski also noted that a bit of graphite powder improves his yields, I figured it can't hurt.
I personally don't think it would do much, but it would be remiss of me not to share this fact.

If I were going to do any such work (and I haven't nor am I in any position to do so) I would begin with Silver
Yes, IMO being able to do this sort of work really separates the armchair alchemists from the wizards (nothing wrong with being an armchair alchemist though because we all gotta start somewhere).
I felt so proud after ghetto'ing my own furnace and feeling like I suddenly stepped up to the plate with the big boys.
IMO you need a flame powered furnace which can reach 1000+ celcius (that could be from either propane or charcoal).
Electric furnaces simply won't cut it. In fact IMO it's downright dangerous to have any AC electricity anywhere near a high heat HIM + sulfur reaction [ask me how do I know this :( ].
So, for anyone who will ever try this, please be sure to keep all electrical equipment and cables at least 2 metres away from the reaction zone.
 
Last edited:

Lux Natura

Occultum
Honorable Meister
Hermetic Pilgrim
Joined
Aug 25, 2016
Messages
675
It's extremely easy to separate gold from bismuth with a cupel,

This is the same thing I was thinking. I have been following Jason's work (and many others) for years. You can tell who knows their stuff, and who has their head in the clouds without their feet on the ground. Gold Fever is a real thing, and it has led many down the path of destruction and poverty.

A friend recently retired from gold mining (family run business). They are small timers in comparison to many other operations, but do well enough, and still move massive amounts of earth, reroute rivers, and so on. Some of the most valuable things they have unearthed isn't even gold. Have had many great conversations with him, and he's run into more gold kooks than you can imagine. He's seen his share of people with "interesting" ideas come and go over the years - almost all of them basically fail and go bankrupt.

There's an interesting geological anomaly in the area their family mines - and all the gold miners surround this area. It is a low-laying singular mountain that had a dome that collapsed. Over the decades, he says many have come to study the feature, with all manner of equipment. They have done test drills. No gold has been found in the mountain, but the rivers that run off from there have deposited gold in the surrounding areas. Back in the early 1980's they paid over $175k to have proper geological reports done on the area. All of their gold is sold to a single Asian cash buyer.

The right type of black sands can contain small amounts of gold and other precious metals - this has been known forever. The question is always whether it is worth it or not to extract it. There is no shortage of precious metals in any case, it is only a matter of economics whether it is worth it or not to work it.
 

Vladimirv

Terrae
Hermetic Pilgrim
Joined
Dec 7, 2025
Messages
152
Link drjoechampion.com/2010 Notes.htm



November 12, 2010 Going all the way

Many have dreamed of this happening and now it is here. I have made a 100% conversion of copper into gold. You read it right I did not say 90% c0nversion of copper into gold I said 100%. Look at all of the metal shown below on my Birthday 11/4/2010. It took about a week for me to developed the refine process, this equates to the final stage of this LENC process. With a little bit of luck and being in the Blue Zone. I can safely say that everything preformed better than I would ever would have engaged. All it took was good science. I would of been satisfied with 10% conversion of the copper by weight but when I took a final review at 4am this morning I was pleasantly surprized that I had 100% conversion. There is 88 bars in the container below. Following is the breakdown as far as today's value.

First picture of the pure gold recovered during last night.


IMGA0059.JPG



MVC-001S.JPG




In my opinion, they placed an electrolyte solution containing ORMUS particles between two copper electrodes and applied a direct current.
To grow, ORMUS needs to absorb free electrons in its spherical clusters. This source provides these electrons. The copper or silver electrodes themselves provide a source of nucleons for the reaction within the ORMUS spherical clusters.

Try repeating this with your metal.
You'll need to adjust the current and voltage.
Ozone is formed during the electrolysis of water.
The electrolyte solution must be pre-saturated with a large amount of ORMUS particles isolated from black sands.
It is also highly advisable to collect "flying" ORMUS from the air overnight and add it to the electrolyte.
 
Last edited:

Vladimirv

Terrae
Hermetic Pilgrim
Joined
Dec 7, 2025
Messages
152
The ORMUS trap can be made from night air using ultrasonic water mist generators.



A large plastic big bag can (100-200L ) be used as a fog collector.
Water collected in the bag should not come into contact with metals.

When water is atomized into a mist by ultrasound, it becomes negatively charged. If you measure its pH with an electronic meter, it will show a pH of 8-9.
Of course, there's no actual pH there; it's just a charge.

This water effectively captures ORMUS from the air, as it is attracted to negatively charged droplets.
This is similar to collecting dew.
Collect only at night, preferably when the moon is visible. Collection is especially effective during a full moon.
The device should operate outdoors or draw in air from outside.
You can add a small amount of water with silver ions to the water in the container with the ultrasonic atomizer. This water can be made by electrolyzing silver in water. Silver ions also effectively attract ORMUS particles from the air and fix them.
 

Andro

Alchemical Adept
Magus de Moderatio
Patron of the Arts
Honorable Meister
Hermetic Pilgrim
Joined
Dec 10, 2009
Messages
8,263
@Vladimirv

Thanks for sharing this!

The device in the video, is it basically a fan-powered air sucker, with the night air going into the water inside the plastic container + ultrasonic atomizer and coming out as negatively charged fog which we collect in a separate container? Am I getting this right?

The starting water in the plastic container is just regular water?

The negative charge of the "fog" is a result of the ultrasonic agitation?
 

Lakshmana

Lapidem
Patron of the Arts
Hermetic Pilgrim
Joined
Jan 24, 2022
Messages
1,081
Are you sure your mist water is 7 pH and not 8-9 from the start? This probably shouldn't produce oh- but if it does that's neat and I'll build it.
 

Lakshmana

Lapidem
Patron of the Arts
Hermetic Pilgrim
Joined
Jan 24, 2022
Messages
1,081
I got the same measurement using distilled water in a jar measured 7pH then run the mister sealed circulation and it's now at 8.5-9 pH
 

Appleheads

Terrae
Hermetic Pilgrim
Joined
Jan 5, 2024
Messages
231
@Vladimirv

Thanks so much for the link and pictures. Such a cool rabbit hole to peruse.

@Lakshmana
Thanks for the results, water is a strange and mysterious substance. I learn more everyday and realize how little I truly don't grasp.
 

Vladimirv

Terrae
Hermetic Pilgrim
Joined
Dec 7, 2025
Messages
152
@Vladimirv

Thanks for sharing this!

The device in the video, is it basically a fan-powered air sucker, with the night air going into the water inside the plastic container + ultrasonic atomizer and coming out as negatively charged fog which we collect in a separate container? Am I getting this right?

The starting water in the plastic container is just regular water?

The negative charge of the "fog" is a result of the ultrasonic agitation?
Yes, you got it right.

I also sometimes add silver ions to the water; they further bind to the ORMUS.

I read on forums discussing growing plants in greenhouses. They use mist irrigation after ultrasound. It significantly accelerates plant growth and yield, and reduces disease.

This is a clear sign that the water is absorbing ORMUS.

When spraying water mechanically, this effect on plants does not occur; only ultrasound does.
 

ghetto alchemist

Hermes Trismegistus
Honorable Meister
Hermetic Pilgrim
Joined
Mar 21, 2011
Messages
1,537
It turns out that pre-charging your magnetite like this is not only desired, BUT CRUCIAL.
I hadn't realised the importance until now, but the magnetite I was using for this had been pre-charged with ~5 cycles of the bion pack process.
[I did each cycle by a single night in the freezer and then heat under LPG for ~1 hour during the day].
Subsequent session/s, with un-treated magnetite in the PRAGG, just don't hit the same.

So for anyone wanting to replicate please make sure to pre-energise your magnetite the same way.
I think the easiest way to do it is to alternate between freezer time and putting in a microwave oven.
(BS:lye:borax:silica:bismuth -> 4:4:4:2:1)
L> + copper sulfate ~0.5
Figured that I should probably update the thread with what I currently know.
I did end up ghetto'ing a high temperature gas furnace which easily gets up to 1000+ degrees celcius.
It also holds a large graphite crucible.
So I ended up running a smelt with the above ratios based on 300 grams of magnetite black sand, according to what was shown in the video [it may or may not have made a difference, but for what it's worth I ran the smelt during the daytime of a new moon].
[I also added copper sulfate, expecting it to decompose into SO2 from the molten lye, according to popcorn theory]
[It's also expected that the same lye will partially dissolve the outside layer of magnetite exposing the HIM center to SO2 (also according to popcorn theory)].


The result was a very heavy button of bismuth.
there is one ingredient which I add to the smelt which I didn't mention.
And that is a sprinkle of flour, not much
Just 1 update to this process.
Everything above is good.
Even the flour, it actually improves yields.

I been previously doing this on the new moon because of a fear of creating DOR type radiation during other moon phase times.
But I recently busted out and tried it outside of the new moon...and guess what....no DOR gets generated...but also, the smelt doesn't work.
The yield goes to total shit....you get almost nothing...just as the muggles expect.
It's totally blown my mind, even after researching alchemy for nearly 20 years, I still didn't actually expect that.
I had to think about it and realised it shouldn't have been a surprise.
Even I myself once said the following:
The moon's affect on alchemy is already well described, all you need to do is to collect your dew on a full moon, and perform your transmutations on the new moon.
I wrote this because I have previously read about only doing transmutation on the new moon in multiple texts, even a first hand testimony about the fact from Terry:
I have noticed the moon has great affects on my work.
If any of you can tell me what astrological information occurred last night 10 - 4-2002 3:00 pm till this morning 10 -5-2002 . 8:00 am .
But even with the weight of such strong textual proof, my puny brain still couldn't accept and understand this simple fact.
But now after seeing with my own eyes, finally I do:
It turns out that Terry was right, indeed the moon has great effects.
Even the smallest amount of moonlight neutrinos will stop the transmutation popcorn reaction from occuring.

I think it goes without saying....if you want to replicate this to get big yields of precious metals...do the smelt on the new moon.
 
Last edited: